Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 60000 V @Thickness 1.57 mm |
60000 V @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S/S |
Industrial Laminates/Norplex NP130HF Glass Fabric Description: High flexural, impact and tensile strength glass fabric epoxy laminate, especially in the machine direction. Engineered to provide better physical properties than NEMA FR-4. More dimens.. |
|||
Dielectric Breakdown | 60000 V @Thickness 1.57 mm |
60000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP511 Glass Fabric Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat.. |
|||
Dielectric Breakdown | 60000 V @Thickness 1.57 mm |
60000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP600 Paper Base Laminate Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. This material is most commonly used for drill entry material in the PCB industry. Thickness Tested: 0.062".. |
|||
Dielectric Breakdown | 60000 V @Thickness 1.57 mm |
60000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP602 Paper Base Laminate Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. It is typically hot punched for numerous low voltage, less than 250 volts, electrical applications.Thickne.. |
|||
Dielectric Breakdown | 60000 V @Thickness 1.57 mm |
60000 V @Thickness 0.0620 in |
Condition A |
Industrial Laminates/Norplex NP631 Paper Base Laminate Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500" |
|||
Dielectric Breakdown | 60000 V @Thickness 1.57 mm |
60000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP664 Paper Base Laminate Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062.. |