Polymer Property : Electrical Resistivity = 0.00200 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.000300 - 0.00200 ohm-cm

@Temperature 65.0 - 150 °C
0.000300 - 0.00200 ohm-cm

@Temperature 149 - 302 °F
Average value: 0.00364 ohm-cm Grade Count:2
Overview of materials for Epoxy, Electrically Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of..