Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000154 ohm-cm | 0.000154 ohm-cm | |
ATI Wah Chang 425™ Titanium Alloy, Annealed Bar 0.5 - 1.23 in. dia ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Electrical Resistivity | 0.000154 ohm-cm | 0.000154 ohm-cm | |
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Electrical Resistivity | 0.000154 ohm-cm | 0.000154 ohm-cm | |
ATI Wah Chang 425™ Titanium Alloy, Solution Treated Annealed Bar 0.5 - 1.23 in. dia ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Electrical Resistivity | 0.000154 ohm-cm | 0.000154 ohm-cm | |
ATI Wah Chang 425™ Titanium Alloy, Tubular Extruded ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Electrical Resistivity | 0.000154 ohm-cm | 0.000154 ohm-cm | |
ATI Wah Chang 425™ Titanium Alloy, Tubular Extruded, Mill Annealed ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Electrical Resistivity | 0.000154 ohm-cm | 0.000154 ohm-cm | |
ATI Wah Chang 425™ Titanium Alloy, Cold Rolled Sheet ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Electrical Resistivity | 0.000154 ohm-cm | 0.000154 ohm-cm | |
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate, Solution Treated Annealed ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |