Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000142 ohm-cm @Temperature 700 °C |
0.000142 ohm-cm @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 700 °C |
0.000142 ohm-cm @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 700 °C |
0.000142 ohm-cm @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 700 °C |
0.000142 ohm-cm @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 700 °C |
0.000142 ohm-cm @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Electrical Resistivity | 0.000142 ohm-cm | 0.000142 ohm-cm | |
Goodfellow Cobalt/Silicon/Boron/Iron/Nickel Alloy Metallic glasses (glassy alloys) or amorphous metals. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.Information provided by Goodfellow. |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 55F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F) Not listed in the ASTM.Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Grade 45 Type 1 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Grade 55 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1018, Grade 30 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1018, Grade 33 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 1 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 1 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 1 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 1 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Grade 33 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Grade 36 Type 1 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Grade 36 Type 2 Hot Rolled Carbon Steel, Structural Steel (SS) Type 2 for conversion to A36Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Grade 40 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 20.0 °C |
0.000142 ohm-cm @Temperature 68.0 °F |
|
AK Steel ASTM A 568 and A 635 Hot Rolled Carbon Steel, Structural Steel (SS) For conversion to A36 plateInformation provided by AK Steel |
|||
Electrical Resistivity | 0.000142 ohm-cm @Temperature 700 °C |
0.000142 ohm-cm @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |