Polymer Property : Electrical Resistivity = 0.000138 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.000138 ohm-cm

@Temperature 600 °C
0.000138 ohm-cm

@Temperature 1110 °F
Haynes 625 alloy, 10% cold reduction, 1010°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 700 °C
0.000138 ohm-cm

@Temperature 1290 °F
Haynes 625 alloy, 20% cold reduction, 1065°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 600 °C
0.000138 ohm-cm

@Temperature 1110 °F
Haynes 625 alloy, 20% cold reduction, 1120°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 600 °C
0.000138 ohm-cm

@Temperature 1110 °F
Haynes 625 alloy, 20% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 700 °C
0.000138 ohm-cm

@Temperature 1290 °F
Haynes 625 alloy, 20% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 700 °C
0.000138 ohm-cm

@Temperature 1290 °F
Haynes 625 alloy, 30% cold reduction, 1065°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 600 °C
0.000138 ohm-cm

@Temperature 1110 °F
Haynes 625 alloy, 30% cold reduction, 1120°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 600 °C
0.000138 ohm-cm

@Temperature 1110 °F
Haynes 625 alloy, 30% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 600 °C
0.000138 ohm-cm

@Temperature 1110 °F
Haynes 625 alloy, 40% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 600 °C
0.000138 ohm-cm

@Temperature 1110 °F
Haynes 625 alloy, 50% cold reduction, 1010°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 600 °C
0.000138 ohm-cm

@Temperature 1110 °F
Haynes 625 alloy, 50% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 700 °C
0.000138 ohm-cm

@Temperature 1290 °F
Haynes 625 alloy, cold rolled and 1050°C mill-annealed sheet
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 700 °C
0.000138 ohm-cm

@Temperature 1290 °F
Haynes 625 alloy, plate after 1000 hours at 650°C (1200°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 700 °C
0.000138 ohm-cm

@Temperature 1290 °F
Haynes 625 alloy, plate after 1000 hours at 760°C (1400°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 700 °C
0.000138 ohm-cm

@Temperature 1290 °F
Haynes 625 alloy, plate after 16000 hours at 650°C (1200°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 600 °C
0.000138 ohm-cm

@Temperature 1110 °F
Haynes 625 alloy, plate after 16000 hours at 870°C (1600°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 700 °C
0.000138 ohm-cm

@Temperature 1290 °F
Haynes 625 alloy, plate after 16000 hours at 870°C (1600°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 600 °C
0.000138 ohm-cm

@Temperature 1110 °F
Haynes 625 alloy, plate after 8000 hours at 650°C (1200°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 700 °C
0.000138 ohm-cm

@Temperature 1290 °F
Haynes 625 alloy, plate after 8000 hours at 650°C (1200°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 700 °C
0.000138 ohm-cm

@Temperature 1290 °F
Haynes 625 alloy, plate after 8000 hours at 760°C (1400°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 600 °C
0.000138 ohm-cm

@Temperature 1110 °F
Haynes 625 alloy, plate after 8000 hours at 870°C (1600°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 300 °C
0.000138 ohm-cm

@Temperature 572 °F
Haynes Hastelloy® B-3® alloy, 20% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 400 °C
0.000138 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® B-3® alloy, 20% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 300 °C
0.000138 ohm-cm

@Temperature 572 °F
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 400 °C
0.000138 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 400 °C
0.000138 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® B-3® alloy, 6.3 mm plate
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 600 °C
0.000138 ohm-cm

@Temperature 1110 °F
Haynes 625 alloy, 30% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 600 °C
0.000138 ohm-cm

@Temperature 1110 °F
Haynes 625 alloy, 10% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 600 °C
0.000138 ohm-cm

@Temperature 1110 °F
Haynes 625 alloy, 40% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
Electrical Resistivity 0.000138 ohm-cm

@Temperature 700 °C
0.000138 ohm-cm

@Temperature 1290 °F
Haynes 625 alloy, 40% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..