Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000920 ohm-cm | 0.0000920 ohm-cm | RT |
Outokumpu 4565 High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Electrical Resistivity | 0.0000920 ohm-cm | 0.0000920 ohm-cm | |
Outokumpu 4724 High Temperature Ferritic Stainless Steel Truly stainless high temperature grade with 13% chromium. Not critical in terms of embrittlement.Applications: Mostly used in high temperature applications with sulphurous atmospheres and/or low te.. |