Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000580 ohm-cm | 0.0000580 ohm-cm | Temp Coefficient 0.0011/ºC (-17.8-449ºC) |
Carpenter HyMu "80"® Electronic Alloy, Cold Rolled Strip Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Electrical Resistivity | 0.0000580 ohm-cm | 0.0000580 ohm-cm | Temp Coefficient 0.0011/ºC (-17.8-449ºC) |
Carpenter HyMu "80"® Electronic Alloy, Bar, After Process Anneal Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Electrical Resistivity | 0.0000580 ohm-cm | 0.0000580 ohm-cm | Temp Coefficient 0.0011/ºC (-17.8-449ºC) |
Carpenter HyMu "80"® Electronic Alloy, Cold Drawn Bar Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Electrical Resistivity | 0.0000580 ohm-cm | 0.0000580 ohm-cm | Temp Coefficient 0.0011/ºC (-17.8-449ºC) |
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Bar Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Electrical Resistivity | 0.0000580 ohm-cm | 0.0000580 ohm-cm | Temp Coefficient 0.0011/ºC (-17.8-449ºC) |
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Strip Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Electrical Resistivity | 0.0000580 ohm-cm | 0.0000580 ohm-cm | Temp Coefficient 0.0011/ºC (-17.8-449ºC) |
Carpenter HyMu "80"® Electronic Alloy, Strip, After Process Anneal Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |