Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00400 - 0.00700 ohm-cm | 0.00400 - 0.00700 ohm-cm | |
Alliance BIN-40 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00400 - 0.00700 ohm-cm | 0.00400 - 0.00700 ohm-cm | |
Alliance BIN-26 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00400 - 0.00700 ohm-cm | 0.00400 - 0.00700 ohm-cm | |
Alliance BIN-45 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00400 - 0.00700 ohm-cm | 0.00400 - 0.00700 ohm-cm | |
Alliance BIN-48 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00400 - 0.00700 ohm-cm | 0.00400 - 0.00700 ohm-cm | |
Alliance BIN-55 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00400 - 0.00700 ohm-cm | 0.00400 - 0.00700 ohm-cm | |
Alliance BIN-72 Bonded (Composite) Magnetic Material |