Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-28EH Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-28UH Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-30EH Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-30UH Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-35 Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-35H Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-35M Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-35SH Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-35UH Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-38 Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-38SH Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-40H Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-40M Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-40SH Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-42 Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-42M Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-42SH Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-44H Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-45 Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-45M Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-50 Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-30EZ Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-33 Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-33H Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-33UH Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-38M Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-40 Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-42H Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-33M Neodymium Iron Boron Magnetic Material
|
Electrical Resistivity |
0.000120 - 0.000160 ohm-cm |
0.000120 - 0.000160 ohm-cm |
|
Alliance N-48 Neodymium Iron Boron Magnetic Material
|