Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 165 Forgings & Extrusions; A (TB00) Temper (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; over 25 to 51 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 165 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 165 Rod and Bar; H (TD04) Temper; over 25.4 to 76 mm (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 165 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 165 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 51 to 76 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 9.5 to 25 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; over 25.4 to 76 mm (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Strip; 1/2H (TD02) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.5Formability Ratio (bad Way): 1Superficial Hardness: 30T 74-79Tabulated properties appl.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Strip; A -Dead Soft (TB00) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 46-67Tabulated properties apply .. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Strip; A -Planished (TB00) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 46-67Tabulated properties apply .. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; 0ver 25.4 to 76 mm o.d. (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; over 9.5 to 25.4 mm o.d. (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; up to 9.5 mm o.d. (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Wire; 1/2H (TD02) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Wire; 1/4H (TD01) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Wire; 1/2H (TD02) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Wire; 1/4H (TD01) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 25 to 51 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Rod and Bar; H (TD04) Temper; over 25.4 to 76 mm (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Wire; 3/4H (TD03) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Electrical Resistivity | 0.00000910 - 0.0000115 ohm-cm | 0.00000910 - 0.0000115 ohm-cm | 15-19% IACS Conductivity |
Materion Beryllium Copper Alloy M25 Wire; H (TD04) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |