Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 5.30e+15 ohm-cm | 5.30e+15 ohm-cm | ASTM D257 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2590 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |
|||
Electrical Resistivity | 5.30e+15 - 3.00e+16 ohm-cm | 5.30e+15 - 3.00e+16 ohm-cm | Average value: 2.18e+16 ohm-cm Grade Count:3 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |