Electrical Properties Metric English Comments
Electrical Resistivity 0.000142 ohm-cm

@Temperature 700 °C
0.000142 ohm-cm

@Temperature 1290 °F
Haynes Hastelloy® B-3® alloy, 20% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000142 ohm-cm

@Temperature 700 °C
0.000142 ohm-cm

@Temperature 1290 °F
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000142 ohm-cm

@Temperature 700 °C
0.000142 ohm-cm

@Temperature 1290 °F
Haynes Hastelloy® B-3® alloy, 30% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000142 ohm-cm

@Temperature 700 °C
0.000142 ohm-cm

@Temperature 1290 °F
Haynes Hastelloy® B-3® alloy, 40% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000142 ohm-cm

@Temperature 700 °C
0.000142 ohm-cm

@Temperature 1290 °F
Haynes Hastelloy® B-3® alloy, 50% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000142 ohm-cm

@Temperature 700 °C
0.000142 ohm-cm

@Temperature 1290 °F
Haynes Hastelloy® B-3® alloy, 6.3 mm plate
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Electrical Resistivity 0.000142 ohm-cm
0.000142 ohm-cm
Goodfellow Cobalt/Silicon/Boron/Iron/Nickel Alloy
Metallic glasses (glassy alloys) or amorphous metals. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.Information provided by Goodfellow.
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 1011, Class 2 Formable, Grade 55F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F)
Not listed in the ASTM.Information provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 1011, Grade 45 Type 1 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 1011, Grade 50 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 1011, Grade 55 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 1018, Grade 30 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 1018, Grade 33 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 1011, Class 1 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA)
Information provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 1011, Class 1 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA)
Information provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 1011, Class 1 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA)
Information provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 1011, Class 2 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA)
Information provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 1011, Grade 30 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 1011, Grade 33 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 1011, Grade 36 Type 1 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 1011, Grade 36 Type 2 Hot Rolled Carbon Steel, Structural Steel (SS)
Type 2 for conversion to A36Information provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 1018, Grade 40 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 20.0 °C
0.000142 ohm-cm

@Temperature 68.0 °F
AK Steel ASTM A 568 and A 635 Hot Rolled Carbon Steel, Structural Steel (SS)
For conversion to A36 plateInformation provided by AK Steel
Electrical Resistivity 0.000142 ohm-cm

@Temperature 700 °C
0.000142 ohm-cm

@Temperature 1290 °F
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched