Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000670 ohm-cm @Temperature 23.0 °C |
0.0000670 ohm-cm @Temperature 73.4 °F |
|
Crucible Steel 446 Chromium Steel Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi.. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201, 10% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201, 40% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201, 5% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201, 50% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201, 60% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201L, 10% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201L, 20% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201L, 5% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201L, 50% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201L, 60% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201L, Annealed (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201, 20% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201, 30% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201, Annealed (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201L, 30% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Electrical Resistivity | 0.0000670 ohm-cm | 0.0000670 ohm-cm | |
ATI Allegheny Ludlum Stainless Steel Type 201L, 40% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |