Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000318 ohm-cm | 0.00000318 ohm-cm | Annealed |
Eagle Brass 210 Gilding Metal, 1/2 Hard CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Electrical Resistivity | 0.00000318 ohm-cm | 0.00000318 ohm-cm | Annealed |
Eagle Brass 210 Gilding Metal, 1/4 Hard CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Electrical Resistivity | 0.00000318 ohm-cm | 0.00000318 ohm-cm | Annealed |
Eagle Brass 210 Gilding Metal, 3/4 Hard CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Electrical Resistivity | 0.00000318 ohm-cm | 0.00000318 ohm-cm | Annealed |
Eagle Brass 210 Gilding Metal, Annealed CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Electrical Resistivity | 0.00000318 ohm-cm | 0.00000318 ohm-cm | Annealed |
Eagle Brass 210 Gilding Metal, Extra Hard CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Electrical Resistivity | 0.00000318 ohm-cm | 0.00000318 ohm-cm | Annealed |
Eagle Brass 210 Gilding Metal, Extra Spring CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Electrical Resistivity | 0.00000318 ohm-cm | 0.00000318 ohm-cm | Annealed |
Eagle Brass 210 Gilding Metal, Hard CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Electrical Resistivity | 0.00000318 ohm-cm | 0.00000318 ohm-cm | Annealed |
Eagle Brass 210 Gilding Metal, Spring CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |