Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 110 EPT COPPER, 1/2 Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 110 EPT COPPER, 1/4 Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 110 EPT COPPER, 3/4 Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 110 EPT COPPER, Annealed Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 110 EPT COPPER, Extra Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 110 EPT COPPER, Extra Spring Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 110 EPT COPPER, Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 110 EPT COPPER, Spring Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 101 OFE COPPER (Certified), 1/2 Hard Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 101 OFE COPPER (Certified), 3/4 Hard Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 101 OFE COPPER (Certified), Annealed Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 101 OFE COPPER (Certified), Extra Hard Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 101 OFE COPPER (Certified), Extra Spring Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 101 OFE COPPER (Certified), Hard Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 101 OFE COPPER (Certified), Spring Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 102 OF COPPER (Non-Certified), 1/2 Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 102 OF COPPER (Non-Certified), 1/4 Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 102 OF COPPER (Non-Certified), 3/4 Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 102 OF COPPER (Non-Certified), Annealed Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 102 OF COPPER (Non-Certified), Extra Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 102 OF COPPER (Non-Certified), Extra Spring Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 102 OF COPPER (Non-Certified), Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 102 OF COPPER (Non-Certified), Spring Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Electrical Resistivity | 0.00000176 ohm-cm | 0.00000176 ohm-cm | Annealed |
Eagle Brass 101 OFE COPPER (Certified), 1/4 Hard Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Electrical Resistivity | <= 0.00000176 ohm-cm | <= 0.00000176 ohm-cm | Calculated from Min 98 %IACS |
Cadi C10100 Oxygen Free Copper Oxygen Free Copper is specified when resistance to hydrogen embrittlement is required due to application in a high temperature, hydrogen environment.Forms: RodBarPlateInformation provided by Cadi Co.. |
|||
Electrical Resistivity | <= 0.00000176 ohm-cm | <= 0.00000176 ohm-cm | Calculated from Min 98 %IACS |
Cadi C11000 ETP Standard Grade Copper The standard grade of copper - most widely used electrical conductor - suitable where mechanical design is not an issue and maximization of electrical or thermal conductivity is the primary concern... |