Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 270 - 295 °C | 518 - 563 °F | Injection Molding |
LG Chemical LUMID EG2309B(W) PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol) Feature: Injection Molding, PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)Application: Radiator Tank, Intercooler TankCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG .. |
|||
Melt Temperature | 270 - 295 °C | 518 - 563 °F | Injection Molding |
LG Chemical LUMID GP2430B(W) PA66+GF43%, General Purpose Feature: Injection Molding, PA66+GF43%, General PurposeApplication: Automotive (Air Intake Manifold)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Melt Temperature | 275 - 295 °C | 527 - 563 °F | |
Lavergne VYPET VNT 615 FR PET 15% Glass Reinforced, Flame Retardant Vypet VNT 615 FR is a 15% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216.. |
|||
Melt Temperature | 275 - 295 °C | 527 - 563 °F | Recommended |
Lanxess Durethan® A 30 H3.0 000000 Nylon 66 PA 66, non reinforced, injection molding, heat-ageing stabilized |
|||
Melt Temperature | 270 - 295 °C | 518 - 563 °F | |
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 270 - 295 °C | 518 - 563 °F | |
A. Schulman SCHULAMID® 6 GF35 35% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 270 - 295 °C | 518 - 563 °F | |
A. Schulman SCHULAMID® 6 GB30 30% Glass Bead Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 270 - 295 °C | 518 - 563 °F | |
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 270 - 295 °C | 518 - 563 °F | |
A. Schulman SCHULAMID® 6 GF35 35% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 275 - 295 °C | 527 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 CF10 HWCP 10% Carbon Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 15 HWCP 15% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 25 DCHP 25% Glass Fiber Nylon 66, Special Heat Ageing Stabilization, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 30 HW 30% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 35 HWCP 35% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 35 HWCP 35% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 40 HWCP 40% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 45 HWCP 45% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 MR 409 HWCP 40% Mineral Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 270 - 295 °C | 518 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 MRGV 20/20 HWCP 20% Mineral and 20% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 270 - 295 °C | 518 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 295 °C | 509 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 MZ 315 CP Combination Nylon 66, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 260 - 295 °C | 500 - 563 °F | |
CP-Polymer-Technik Wellamid® 6600 PA-66-HWL UL-Licensed Nylon 66, Flame Protection Grade V-2, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 270 - 295 °C | 518 - 563 °F | |
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, .. |
|||
Melt Temperature | 270 - 295 °C | 518 - 563 °F | |
BASF Ultramid® TG3S BK 5966 15% Glass Filled PA6 (Conditioned) Description: Ultramid TG7S Bk-102 is a 34% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the.. |