Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 177 - 187 °C | 351 - 369 °F | |
Huntsman PE1407 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |