Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
PolyOne Geon™ Vinyl Wire & Cable E 1400 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
PolyOne Geon™ Vinyl Wire & Cable E1330I Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
PolyOne Geon™ Vinyl Wire & Cable EC486 DA Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
PolyOne Geon™ Vinyl Wire & Cable JC837DB Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
PolyOne Geon™ Vinyl Wire & Cable L00221 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJCK504L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
PolyOne Geon™ Vinyl Wire & Cable WR8180L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
Petroquimica Triunfo Trithene® SX 7012 LDPE - Blow Molding The Trithene SX 7012 resin is a low density polyethylene (LDPE) with medium molecular weight which allows the production of flasks with an adequate combination of mechanical and impact strength, fle.. |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
PolyOne Geon™ Vinyl Flexible R7543E Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
PolyOne Geon™ Vinyl Flexible R7545H Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
PolyOne Geon™ Vinyl Flexible R7661A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
PolyOne Geon™ Vinyl Flexible R7831A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
PolyOne Geon™ Vinyl Flexible R8180K Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 160 - 175 °C | 320 - 347 °F | |
SABIC HP4023W Low Density Polyethylene for Blown Film Product Description: HP4023W is a Low Density Polyethylene grade suitable for producing general purpose films and contains slip and antiblock additives. It yields excellent processability with goo.. |
|||
Melt Temperature | 160 - 175 °C | 320 - 347 °F | blown film equipment |
DuPont Nucrel® 30707SR Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
(discontinued **) 7 wt% Acrylic Acid.Nucrel® 30707SR is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio.. |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
PolyOne Geon™ Vinyl Flexible R3792C Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
PolyOne Geon™ Vinyl Flexible R3792E Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
PolyOne Geon™ Vinyl Flexible R8206A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
Lucobit Lucofin® 7410 HFFR EBA MDH Cable Sheathing Lucofin® 7410 HFFR is a thermoplastic, halogen free flame retardant and low smoke compound for the insulation and/ or sheathing of cables. This grade is based on ethylene butyl acrylate (EBA) and.. |
|||
Melt Temperature | 125 - 175 °C | 257 - 347 °F | blown film extrusion |
DuPont Elvax® 3170 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3170 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melt Temperature | 125 - 175 °C | 257 - 347 °F | blown film extrusion |
DuPont Elvax® 3170SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3170SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res.. |
|||
Melt Temperature | 160 - 175 °C | 320 - 347 °F | blown film equipment |
DuPont Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating 7 wt% Acrylic Acid.Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion .. |
|||
Melt Temperature | 150 - 175 °C | 302 - 347 °F | Blown Film Coextrusion |
DuPont™ Elvax® 3169Z Ethylene Vinyl Acetate DuPont™ Elvax® 3169Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3.. |
|||
Melt Temperature | 165 - 175 °C | 329 - 347 °F | |
EMS-Griltech Grilene® KE 170 CoPES Mono-Component Fusible Adhesive Fiber Description: Grilene KE 170 is the higher melting CoPES mono-component fusible adhesive fiber. It is used in compact dry-laid nonwoven.Data provided by EMS-Griltech. |
|||
Melt Temperature | 150 - 175 °C | 302 - 347 °F | |
DuPont Elvax® 3128 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 8.9 wt% Vinyl Acetate.Elvax® 3128 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resin.. |