Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable 0650-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable JJF102L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable MJF114A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1104L-xx40D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1250L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJJX207L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 143 - 171 °C | 289 - 340 °F | |
PolyOne Versaflex™ CL2003X Thermoplastic Elastomer (TPE) Versaflex™ CL2003X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and ultra-soft properties are desired. New Product. Commercial specifications ha.. |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCG20BK Copolymer PP, 20% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCG30BK Copolymer PP, 30% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCG40BK Copolymer PP, 40% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCM10BK Copolymer PP Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCM6BK Copolymer PP Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCT40BK Copolymer PP, 40% Talc Filled Information provided by Niche Polymer |
|||
Melt Temperature | 168 - 171 °C | 334 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJAF111L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Huntsman PE1023 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good draw down characteristics.Applications: Film extrusion: drum liners, hardware packaging, and refuse bags.FDA Notes: Conforms to FDA regulation 21 CFR 17.. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 8925-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 8940-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 8950-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 8960-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 8980-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 8999-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 9077-70 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 9600-70 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 9915-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 9925-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 9940-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 9960-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 9980-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Huntsman PE1059 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down and good processability.Applications: Film extrusion: non-abrasive packaging applications.FDA Notes: Conforms to FDA regulation 21 CFR 177.. |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable 1721-xx14E Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |