Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 163 - 168 °C | 325 - 334 °F | |
PolyOne Geon™ Vinyl Wire & Cable 0860-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 163 - 168 °C | 325 - 334 °F | |
PolyOne Geon™ Vinyl Wire & Cable 2510-xx05D Polyvinyl Chloride Alloy (PVC Alloy) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 163 - 168 °C | 325 - 334 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJLF112L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 163 - 168 °C | 325 - 334 °F | |
PolyOne Geon™ Vinyl Flexible B6000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 160 - 168 °C | 320 - 334 °F | |
PolyOne Geon™ Vinyl Flexible 82024 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Melt Temperature | 163 - 168 °C | 325 - 334 °F | |
PolyOne Geon™ Vinyl Flexible R5145A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |