Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 154 - 160 °C | 309 - 320 °F | |
PolyOne Geon™ Vinyl Wire & Cable 3201-xx05D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Wire & Cable JA306BA Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Wire & Cable JJK501L Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Wire & Cable W2301 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJKC304 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 154 °C | 309 °F | ASTM D789 |
Niche Polymer PA66GF13BK Nylon 66, 13% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJKC302LR Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 154 °C | 309 °F | |
Advanced Elastomer Systems VistaFlex® 641N Thermoplastic Rubber
(discontinued **) A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 7.2 MPa (1050 psi); Vica.. |
|||
Melt Temperature | 154 °C | 309 °F | |
Advanced Elastomer Systems Vistaflex® 671N Thermoplastic Rubber
(discontinued **) A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 9.0 MPa (1300 psi); Vica.. |
|||
Melt Temperature | 154 - 166 °C | 309 - 331 °F | |
PolyOne Geon™ Vinyl Flexible R5160A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |