Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | >= 115 °C | >= 239 °F | |
Polyplastic Armobond® PE 2K Polyethylene Adhesive Compound Information provided by PolyPlastic Group. |
|||
Melt Temperature | 115 - 125 °C | 239 - 257 °F | |
Borealis LE0511 Polyethylene Compound, Crosslinkable, Semiconductive LE0511 is a crosslinkable black polyethylene compound, specially designed for strippable semi conductive screen applications. Applications: LE0511 is intended for strippable outer semi conductive s.. |
|||
Melt Temperature | 115 - 125 °C | 239 - 257 °F | |
Borealis Supersmooth™ LE0504 Crosslinkable Semiconductive Shielding Compound Supersmooth LE0504 is a crosslinkable compound recommended as conductor and bonded insulation shielding for crosslinked polyethylene insulation. Supersmooth LE0504 is based on an ethylene vinyl acet.. |
|||
Melt Temperature | 115 °C | 239 °F | |
Lubrizol Estane® ALR G2000 Water Absorbent Thermoplastic Polyurethane Type: Estane® ALR G2000 is an aliphatic thermoplastic polyurethane (TPU) resin designed to absorb water and transport moisture.Features: Contains UV additivesAvailable in AmericasInformation Provid.. |
|||
Melt Temperature | 115 - 125 °C | 239 - 257 °F | |
Borealis Supersmooth™ LE0500 Crosslinkable Semiconductive Shielding Compound Supersmooth LE0500 is a crosslinkable compound recommended as conductor and bonded insulation shielding for crosslinked polyethylene insulation. Supersmooth LE0500 is based on an ethylene butyl acry.. |
|||
Melt Temperature | 115 - 120 °C | 239 - 248 °F | |
BecauseWeCare BF90 Biodegradable Plastic Biodegradable and compostable product produced from corn and developed to break down within weeks in a compost environment, without leaving any harmful residues in the process. Certified to the vari.. |
|||
Melt Temperature | 115 - 290 °C | 239 - 554 °F | Average value: 191 °C Grade Count:12 |
Overview of materials for Ethylene Butyl Acrylate This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp.. |