Polymer Property : Melt Temperature = 2030 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 1110 - 1280 °C
2030 - 2340 °F
Wieland Duo Pal 6 PFM Alloy
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental
Melt Temperature 1110 - 1200 °C
2030 - 2190 °F
Wieland Porta P6 PFM Alloy
Gold-platinum-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, ceramic veneering, acrylic veneeringDental