Polymer Property : Melt Temperature = 932 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 888 - 932 °C
1630 - 1710 °F
Wieland Portadur P2 Casting Alloy
Gold casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneeringDental