Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 354 - 377 °C | 670 - 710 °F | |
Oxford Polymers PEEK 450-INJ-Black PEEK Product Description: Polyetheretherketone, general purpose injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Carbon black Special Characteristics: Precol.. |
|||
Melt Temperature | 343 - 377 °C | 649 - 711 °F | Stock |
PolyOne Stat-Tech™ RA-06CF-07GF/000 EM Polyarylsulfone - 7% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications - Flow Enhanced Grade Data provided by PolyOne. |
|||
Melt Temperature | 343 - 377 °C | 649 - 711 °F | Stock |
PolyOne Stat-Tech™ RA-06CF-09GF/000 Polyarylsulfone - 9% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications
&a Data provided by PolyOne. |
|||
Melt Temperature | 354 - 377 °C | 670 - 710 °F | Molding |
PolyOne Edgetek® PF-30CF/000 Polysulfone, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |