Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 163 - 168 °C | 325 - 334 °F | |
PolyOne Geon™ Vinyl Wire & Cable 0860-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 163 - 168 °C | 325 - 334 °F | |
PolyOne Geon™ Vinyl Wire & Cable 2510-xx05D Polyvinyl Chloride Alloy (PVC Alloy) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 163 - 168 °C | 325 - 334 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJLF112L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 163 - 168 °C | 325 - 334 °F | |
PolyOne Geon™ Vinyl Flexible B6000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 160 - 168 °C | 320 - 334 °F | |
PolyOne Geon™ Vinyl Flexible 82024 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Melt Temperature | 163 - 168 °C | 325 - 334 °F | |
PolyOne Geon™ Vinyl Flexible R5145A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8600-65 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8915-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8925-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8940-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8950-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8960-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8980-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 8999-65 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9077-65 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9600-65 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9915-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9925-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9940-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9950-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9960-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9980-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 157 - 168 °C | 315 - 335 °F | |
Sylvin Technologies 9999-65 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |