Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 349 - 399 °C | 660 - 750 °F | |
LNP ULTEM® SMU6303 Polyetherimide, 5% Glass Fiber Reinforcement, 5% PTFE Lubricant
(discontinued **) Will be UNTW05.Features: Lubricated, High Heat Resistance, Good Wear Resistance, Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provide.. |
|||
Melt Temperature | 349 - 399 °C | 660 - 750 °F | |
Clariant Renol PEEKSP0002 Polyetheretherketone, 30% Glass Fiber Data provided by Clariant Masterbatches |
|||
Melt Temperature | 349 - 399 °C | 660 - 750 °F | |
Clariant Renol PEEKSP003 Polyetheretherketone, Glass Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 349 - 388 °C | 660 - 730 °F | Molding |
PolyOne Lubri-Tech™ RA-15GF/13T Polyethersulfone, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 V0UL 94 (CTI Testing)PolyOne First ChoiceInformation provided by PolyOne Corporation. |