Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 302 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 302 - 329 °C
575 - 625 °F
Polymer Resources PC-G15 Polycarbonate, 15% Glass Reinforced
Polycarbonate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polym..
Melt Temperature 302 - 329 °C
575 - 625 °F
Polymer Resources PC-G20 Polycarbonate, 20% Glass Reinforced
Polycarbonate, 20% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
Melt Temperature 302 - 329 °C
575 - 625 °F
Polymer Resources PC-G20-[color]-1 Polycarbonate, 20% Glass Reinforced with Mold Release
Polycarbonate, 20% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Melt Temperature 302 - 329 °C
575 - 625 °F
Polymer Resources PC-G40 Polycarbonate, 40% Glass Reinforced
Polycarbonate, 40% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
Melt Temperature 302 - 329 °C
575 - 625 °F
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Melt Temperature 302 - 329 °C
575 - 625 °F
Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Melt Temperature 302 - 329 °C
575 - 625 °F
Polymer Resources PC-HM-FR2-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Melt Temperature 302 - 329 °C
575 - 625 °F
Westlake EC474AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC474 is a general-purpose formulation used for extrusion coating and laminating. It can be drawn down to low coating weights, is processable at high speeds, has go..
Melt Temperature 302 - 329 °C
575 - 625 °F
Westlake EC483 Low Density Polyethylene
WESTLAKE low-density polyethylene EC483 is recommended for use in the boardstock coating industry. This resin has low neck-in, good heat sealing properties, and good drawdown characteristics.Applica..