Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Clamp Pressure = 5800 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Clamp Pressure 40.0 - 70.0 MPa
5800 - 10200 psi
[Mpa/cm<sup>2</sup>]
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Clamp Pressure 40.0 - 70.0 MPa
5800 - 10200 psi
[Mpa/cm<sup>2</sup>]
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Clamp Pressure 40.0 - 70.0 MPa
5800 - 10200 psi
[Mpa/cm<sup>2</sup>]
Parker Chomerics PREMIER™ A220-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Clamp Pressure 40.0 - 70.0 MPa
5800 - 10200 psi
[Mpa/cm<sup>2</sup>]
Parker Chomerics PREMIER™ A240-FRHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Clamp Pressure 40.0 - 70.0 MPa
5800 - 10200 psi
[Mpa/cm<sup>2</sup>]
Parker Chomerics PREMIER™ A240-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Clamp Pressure 40.0 - 70.0 MPa
5800 - 10200 psi
[Mpa/cm<sup>2</sup>]
Parker Chomerics PREMIER™ A230-FRHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Clamp Pressure 40.0 - 70.0 MPa
5800 - 10200 psi
[Mpa/cm<sup>2</sup>]
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Viprene™ P80A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P80A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Viprene™ P90A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P90A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Zythane™ 3045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Zythane™ 4045D Thermoplastic Polyurethane Elastomer
Zythane™ 4045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Zythane™ 5045D Thermoplastic Polyurethane Elastomer
Zythane™ 5045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Zythane™ 5050D Thermoplastic Polyurethane Elastomer
Zythane™ 5050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Zythane™ 5060A Thermoplastic Polyurethane Elastomer
Zythane™ 5060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Zythane™ 5090A Thermoplastic Polyurethane Elastomer
Zythane™ 5090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Zythane™ 6045D Thermoplastic Polyurethane Elastomer
Zythane™ 6045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Zythane™ 6055D Thermoplastic Polyurethane Elastomer
Zythane™ 6055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Zythane™ 6065D Thermoplastic Polyurethane Elastomer
Zythane™ 6065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Zythane™ 6090A Thermoplastic Polyurethane Elastomer
Zythane™ 6090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Zythane™ 7045A Thermoplastic Polyurethane Elastomer
Zythane™ 7045A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Zythane™ 7050D Thermoplastic Polyurethane Elastomer
Zythane™ 7050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer
Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Viprene™ G40D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G40D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Clamp Pressure 40.0 - 70.3 MPa
5800 - 10200 psi
Injection
Alliance Polymers Viprene™ P85A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P85A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Copyright © lookpolymers.com All Rights Reserved