Processing Properties | Metric | English | Comments |
---|---|---|---|
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G85A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G85A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G90A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ P75A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P75A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ P90A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P90A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 4045D Thermoplastic Polyurethane Elastomer Zythane™ 4045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 4060A Thermoplastic Polyurethane Elastomer Zythane™ 4060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 4060D Thermoplastic Polyurethane Elastomer Zythane™ 4060D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 4090A Thermoplastic Polyurethane Elastomer Zythane™ 4090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 5045D Thermoplastic Polyurethane Elastomer Zythane™ 5045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 5080A Thermoplastic Polyurethane Elastomer Zythane™ 5080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 6045D Thermoplastic Polyurethane Elastomer Zythane™ 6045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 6050D Thermoplastic Polyurethane Elastomer Zythane™ 6050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 6065D Thermoplastic Polyurethane Elastomer Zythane™ 6065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 6090A Thermoplastic Polyurethane Elastomer Zythane™ 6090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 7050D Thermoplastic Polyurethane Elastomer Zythane™ 7050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 7055D Thermoplastic Polyurethane Elastomer Zythane™ 7055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ G85A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G85A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 7080A Thermoplastic Polyurethane Elastomer Zythane™ 7080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 7075A Thermoplastic Polyurethane Elastomer Zythane™ 7075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Clamp Pressure | 40.0 - 70.3 MPa | 5800 - 10200 psi | Injection |
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer Zythane™ 7085UF is a UV stabilized polyether-based TPU specifically formulated for extrusion applications. It exhibits excellent abrasion resistance and toughness and has good hydrolytic stability,.. |