Processing Properties | Metric | English | Comments |
---|---|---|---|
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1100-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1100-25 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200-15 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-15 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-20 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200-30 Polyester SMC Premi-Glas® 1200-30 is a fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck and Marine body panels and interior structural components where smooth flat surfac.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200H-20 Polyester SMC Premi-Glas® 1200H-20 is a 20% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94HB flame rec.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200H-22 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1201-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1201-20 is a fiberglass reinforced thermoset sheet molding compound for sanitary ware applications such as shower bases and surrounds, bathtubs and vanity tops.Key features and benefits.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2103-20 CR-SX Fiberglass Reinforced Thermoset BMC Premi-Glas® 2103-20 CR-SX is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regu.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2103-22 CRSX Polyester BMC Premi-Glas® 2103-22 CR-SX is a 22% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2103-25 CRSX Polyester BMC Premi-Glas® 2103-25 CR-SX is a 25% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2200-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2200-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Pigmentable for molded-in c.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2200-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2203-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2204-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2204-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2205-20 CRSX Polyester SMC Premi-Glas® 2205-20 CR-SX is a 20% fiberglass reinforced Sheet Molding Compound formulated for condensate pan applications requiring chemical resistance, heat resistance, dimensional stability, we.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2205-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2205-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2206-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3200-20 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-20 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3200-30 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-30 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3404 33% Glass Reinforced SMC Description: Premi-Glas® 3404 is a glass reinforced thermoset sheet molding compound designed for mass transit and high strength flame retardant applications where low smoke and flame are required... |
|||
Clamp Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
Quantum Composites QC-8700 63% Glass Fiber Reinforced Vinyl Ester SMC QC-8700 is a vinyl ester engineered structural composite molding compound for compression molding of components requiring high structural strength. It exhibits unusual toughness, and is suggested f.. |
|||
Clamp Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
Quantum Composites QC-8850 43% Glass Fiber Reinforced Polyester Hybrid SMC QC-8850 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1286 Glass Reinforced SMC Description: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression molding.. |