Processing Properties | Metric | English | Comments |
---|---|---|---|
Annealing Temperature | 1020 - 1100 °C | 1870 - 2010 °F | Quench Annealing |
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Annealing Temperature | 1020 - 1100 °C | 1870 - 2010 °F | Stress Relief Annealing |
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |