Processing Properties | Metric | English | Comments |
---|---|---|---|
Annealing Temperature | 1010 - 1040 °C | 1850 - 1900 °F | Stress Relief Annealing (min. 0.5 h) |
Outokumpu 353MA® High Temperature Austenitic Stainless Steel Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but.. |
|||
Annealing Temperature | 1010 - 1040 °C | 1850 - 1900 °F | Stress Relief Annealing (min. 0.5 h) |
Outokumpu 4828 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Annealing Temperature | 1010 - 1040 °C | 1850 - 1900 °F | Stress Relief Annealing (min. 0.5 h) |
Outokumpu 4833 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Annealing Temperature | 1010 - 1090 °C | 1850 - 2000 °F | Followed by rapid cooling with forced air or water quenching |
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar Description: 303 UGIMA HD™ is a low sulfur version of Ugitech’s improved machining 303 grade. It is designed to provide better metallurgical performance with respect to weldability, corros.. |
|||
Annealing Temperature | 1010 - 1090 °C | 1850 - 2000 °F | Followed by rapid cooling with forced air or water quenching |
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre.. |
|||
Annealing Temperature | 1010 - 1090 °C | 1850 - 2000 °F | followed by rapid cooling with forced air or water quenching |
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar Description: 316/316L UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 316L, except with respect to machinability. 316/316L UGIM.. |
|||
Annealing Temperature | 1010 - 1090 °C | 1850 - 2000 °F | followed by rapid cooling with forced air or water quenching |
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o.. |