Processing Properties | Metric | English | Comments |
---|---|---|---|
Dew Point | -31.7 - -28.9 °C | -25.0 - -20.0 °F | Average value: -30.4 °C Grade Count:9 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Dew Point | -31.7 °C | -25.0 °F | Average value: -31.7 °C Grade Count:4 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Dew Point | -31.7 °C | -25.0 °F | Average value: -31.7 °C Grade Count:15 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Dew Point | -31.7 °C | -25.0 °F | Average value: -31.7 °C Grade Count:10 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Dew Point | -31.7 - -28.9 °C | -25.0 - -20.0 °F | Average value: -29.8 °C Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are .. |
|||
Dew Point | -31.7 °C | -25.0 °F | Average value: -31.7 °C Grade Count:9 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Dew Point | -31.7 °C | -25.0 °F | Average value: -31.7 °C Grade Count:9 |
Overview of materials for Polyphthalamide (PPA), Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a.. |