Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 1200 min @Temperature 190 °C |
20.0 hour @Temperature 374 °F |
|
Humiseal 1A27 Urethane Conformal Coating Humiseal 1A27 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedPasses thermal shock test (MIL-I-46058C)Flammabilit.. |
|||
Cure Time | 1200 min @Temperature 190 °C |
20.0 hour @Temperature 374 °F |
|
Humiseal 1A27LSE Urethane Conformal Coating Humiseal 1A27LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingPasses thermal shock test (MIL-I-46058C).. |
|||
Cure Time | 1200 min @Temperature 190 °C |
20.0 hour @Temperature 374 °F |
|
Humiseal 1A33 Urethane Conformal Coating Humiseal 1A33 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL.. |
|||
Cure Time | 1200 min @Temperature 190 °C |
20.0 hour @Temperature 374 °F |
|
Humiseal 1A33LSE Urethane Conformal Coating Humiseal 1A33LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses ther.. |
|||
Cure Time | 1200 min | 20.0 hour | Tack-Free Time |
3M AC-665 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-665 Class B are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros.. |