Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 5.50 - 13.5 min | 0.0917 - 0.225 hour | t`90; ASTM D2084 |
ExxonMobil Exxon™ 2211 Fast Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is offwhite to amber balesInformation provided by ExxonMobil Chemical |
|||
Cure Time | 5.50 - 11.5 min | 0.0917 - 0.192 hour | t`50; ASTM D2084 |
ExxonMobil Exxon™ 6222 Brominated Star-Branched Butyl Exxon SB Bromobutyl is a brominated copolymer of isobutylene and isoprene, including a styrene block copolymer branching agent.Information provided by ExxonMobil Chemical |
|||
Cure Time | 5.50 min | 0.0917 hour | Curelastmeter |
Daikin DAI-EL G-781 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |