Cure Time 1.33 - 1.67 min
0.0222 - 0.0278 hour
per mm
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color..
Cure Time 0.333 - 1.67 min
0.00555 - 0.0278 hour
Time to Handling
3M Scotch-Weld™ MG1500 PR Medical Grade Instant Adhesive
3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti..
Cure Time 0.333 - 1.67 min
0.00555 - 0.0278 hour
Time to Handling Strength
3M Scotch-Weld™ PR1500 Plastic and Rubber Instant Adhesive
3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates ..