Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 8.00 min @Temperature 155 °C |
0.133 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.5 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 8.00 min @Temperature 149 °C |
0.133 hour @Temperature 300 °F |
|
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 20.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Cure Time | 8.00 min @Temperature 149 °C |
0.133 hour @Temperature 300 °F |
|
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 62A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Cure Time | 8.00 min @Temperature 68.3 °C |
0.133 hour @Temperature 155 °F |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Cure Time | 8.00 - 12.0 min | 0.133 - 0.200 hour | Working time |
ITW Devcon 2 Ton® Epoxy Clear Epoxy, Clear, White Information provided by ITW Devcon |
|||
Cure Time | 8.00 - 10.0 min | 0.133 - 0.167 hour | Fixture time |
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Ultra White Information provided by ITW Devcon |
|||
Cure Time | 8.00 min | 0.133 hour | Tack Free Time |
Shin-Etsu Silicones KE-3494 Silicone, RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Cure Time | >= 8.00 min | >= 0.133 hour | |
Trelleborg Emerson & Cuming Stycast® 906-1 One-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Cure Time | 8.00 min @Temperature 68.3 °C |
0.133 hour @Temperature 155 °F |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Cure Time | 8.00 min @Temperature 160 °C |
0.133 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR Thanecure® ZM MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 8.00 min @Temperature 155 °C |
0.133 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.5 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 8.00 min @Temperature 155 °C |
0.133 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.75 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 8.00 min @Temperature 155 °C |
0.133 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR Sulfur Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
Cure Time | 8.00 min @Temperature 166 °C |
0.133 hour @Temperature 330 °F |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 330ºF Cure Temperature Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 8.00 min @Temperature 155 °C |
0.133 hour @Temperature 311 °F |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, No Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 8.00 min @Temperature 149 °C |
0.133 hour @Temperature 300 °F |
|
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 20.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Cure Time | 8.00 min @Temperature 149 °C |
0.133 hour @Temperature 300 °F |
|
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 30.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Cure Time | 8.00 min @Temperature 149 °C |
0.133 hour @Temperature 300 °F |
|
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 62A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Cure Time | 8.00 - 16.0 min | 0.133 - 0.267 hour | t'90; ASTM D2084 (mod) |
ExxonMobil Chlorobutyl 1066 Rubber Product Description: Exxon™ Chlorobutyl rubber is a copolymer of isobutylene and isoprene. The product has characteristic specific gravity of 0.93. The product form is white to light amber bales.In.. |
|||
Cure Time | 8.00 min | 0.133 hour | t`50, Target; ASTM D2084 |
ExxonMobil Exxon™ 2222 Regular Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product for is white to light amber bales.Information provided by ExxonMobil Chemical |
|||
Cure Time | 8.00 - 14.0 min | 0.133 - 0.233 hour | t`90; ASTM D2084 |
ExxonMobil Exxon™ 6222 Brominated Star-Branched Butyl Exxon SB Bromobutyl is a brominated copolymer of isobutylene and isoprene, including a styrene block copolymer branching agent.Information provided by ExxonMobil Chemical |
|||
Cure Time | 8.00 - 10.0 min | 0.133 - 0.167 hour | Time to Handling Strength |
3M Scotch-Weld™ DP405 LH Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel.. |
|||
Cure Time | 8.00 min @Temperature 155 °C |
0.133 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.75 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 8.00 min @Temperature 155 °C |
0.133 hour @Temperature 311 °F |
TC90 |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR Sulfur Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
Cure Time | 8.00 min @Temperature 166 °C |
0.133 hour @Temperature 330 °F |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 330ºF Cure Temperature Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 8.00 min @Temperature 155 °C |
0.133 hour @Temperature 311 °F |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, No Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 8.00 min @Temperature 149 °C |
0.133 hour @Temperature 300 °F |
|
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 30.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Cure Time | 8.00 - 10.0 min | 0.133 - 0.167 hour | Time to Handling Strength |
3M Scotch-Weld™ DP405 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel.. |