Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6005 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6103 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6105 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6601 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6605 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6704 Adhesive Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal .. |
|||
Cure Time | 480 min | 8.00 hour | Full Cure |
Resinlab® RC8038 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Cure Time | 480 min | 8.00 hour | Full Cure |
Resinlab® RC8041 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Cure Time | 480 min | 8.00 hour | Full Cure |
Resinlab® RC8060 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6004 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6102 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6204 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6801 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6804 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6806 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6810 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6811 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 480 min | 8.00 hour | |
Lord Adhesives 304 General Purpose, High Viscosity Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Cure Time | 480 min | 8.00 hour | |
Lord Adhesives 305 General Purpose, Medium Viscosity Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Cure Time | 480 min | 8.00 hour | 4 hrs @ 25°C + 4 hrs @ 65°C-plus |
Tra-Con Tra-Bond 2114 Water White Transparent Epoxy Adhesive TRA-BOND 2114 is a transparent, low viscosity epoxy resin formulation recommended for industrial adhesive and laminating applications where sparkling clarity and excellent structural, mechanical and.. |
|||
Cure Time | 480 min | 8.00 hour | Tack-Free Time |
3M AC-350 Class A-2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have.. |
|||
Cure Time | 480 - 720 min @Temperature 24.0 °C |
8.00 - 12.0 hour @Temperature 75.2 °F |
|
BCC Products BC 6004 Epoxy Surface Coat BC 6004 is a white thixotropic epoxy surface coat that has the ability to cure and bond to freshly poured wet plaster. This formulated resin compound can be applied with a brush or troweled to a thi.. |
|||
Cure Time | 480 - 1440 min | 8.00 - 24.0 hour | Full Cure |
3M Scotch-Weld™ DP8010 Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl.. |
|||
Cure Time | 480 min | 8.00 hour | 4 hrs @ 25°C + 4 hrs @ 65°C |
Atom Adhesives AA-BOND 2110 Epoxy Adhesive AA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, no.. |
|||
Cure Time | 480 min | 8.00 hour | Hard Dry |
3M Scotchkote™ 474 Epoxy Concrete Repair Scotchkote Epoxy Concrete Repair 474 has been specifically developed as a three component 100% solids high performance mortar for use as a heavy duty repair system for concrete surfaces.Product Feat.. |
|||
Cure Time | 480 min | 8.00 hour | Full Cure |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Cure Time | 480 min | 8.00 hour | Full Cure |
Resinlab® TL5062 Anaerobic Threadlocking Compound The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a .. |
|||
Cure Time | 480 - 1440 min | 8.00 - 24.0 hour | Average value: 880 min Grade Count:3 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |