Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 2.50 - 4.83 min | 0.0417 - 0.0806 hour | Gelation time |
Mitsui MILEXâ„¢ XL-225MB Phenol Aralkyl Resin, Standard Grade The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad.. |
|||
Cure Time | 2.50 - 3.00 min @Temperature 150 °C |
0.0417 - 0.0500 hour @Temperature 302 °F |
|
Loctite® 3607 Pin Transfer Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te.. |
|||
Cure Time | 2.50 - 5.50 min | 0.0417 - 0.0917 hour | ts2; ASTM D2084 |
ExxonMobil Exxon™ 4266 Star-Branched Butyl Exxon SB Butyl is a copolymer of isobutylene and isoprene, including a styrene block copolymer branching agent.Information provided by ExxonMobil Chemical |
|||
Cure Time | 2.50 - 7.50 min | 0.0417 - 0.125 hour | ts2; ASTM D2084 |
ExxonMobil Exxon™ 6222 Brominated Star-Branched Butyl Exxon SB Bromobutyl is a brominated copolymer of isobutylene and isoprene, including a styrene block copolymer branching agent.Information provided by ExxonMobil Chemical |
|||
Cure Time | 2.50 min | 0.0417 hour | Curelastmeter |
Daikin DAI-EL G-801 Fluoroelastomer Copolymer, Peroxide Curable Grade, 66% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good low-temperature and elasticity characteristics.Information provided by Daikin Industries. |
|||
Cure Time | 2.50 min | 0.0417 hour | Set Time |
3M Scotch-Weld™ TE230 Black Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Cure Time | 2.50 min | 0.0417 hour | Set Time |
3M Scotch-Weld™ TS230 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Cure Time | 2.50 min | 0.0417 hour | Set Time |
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th.. |
|||
Cure Time | 2.50 - 5.83 min | 0.0417 - 0.0972 hour | Gelation time |
Mitsui MILEX™ XL-1210MB Phenol Aralkyl Resin, Silicone Rubber Modified
(discontinued **) The MILEX™ Family of products is widely featured in brake systems of automobiles made by the top automakers through Mitsui Chemicals' affiliation with leading brake manufacturers. The phenolic .. |