Processing Properties Metric English Comments
Cure Time >= 0.300 min
>= 0.00500 hour
Fixture
Resinlab® CYNERGY CA6906 Adhesive
Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials..
Cure Time >= 0.300 min
>= 0.00500 hour
Fixture
Resinlab® CYNERGY CA6907 Adhesive
Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials..
Cure Time >= 0.300 min
>= 0.00500 hour
Fixture
Resinlab® CYNERGY CA6404 Adhesive
Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa..
Cure Time >= 0.300 min
>= 0.00500 hour
Fixture
Resinlab® CYNERGY CA6405 Adhesive
Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa..
Cure Time >= 0.300 min
>= 0.00500 hour
Fixture
Resinlab® CYNERGY CA6503 Adhesive
Description: The CYNERGY 6500 SERIES are black, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa..
Cure Time 0.300 min
0.00500 hour
Loctite® 414 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Cure Time 0.300 min
0.00500 hour
Loctite® 420 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Cure Time 0.300 min
0.00500 hour
Loctite® 426 Toughened Ethyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Cure Time 0.300 min
0.00500 hour
Loctite® Super Bonder® 495 Instant Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Cure Time >= 0.300 min
>= 0.00500 hour
Fixture
Resinlab® CYNERGY CA6905 Adhesive
Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials..