Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.250 - 0.583 min | 0.00417 - 0.00972 hour | On Steel (Fixture) |
ND Industries 306 Surface Insensitive Instant Superglue Low viscosity for difficult to bond rubber compounds |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries 331 Surface Insensitive Instant Superglue Medium-high viscosity for difficult to bond surfaces |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries 360 Surface Insensitive Instant Superglue General DescriptionA medium viscosity, general purpose cyanoacrylate which is also surface sensitive. Can handle a wide array of materials which include wood, cork, leather, stone and plastics, in .. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | on metal (Fixture) |
ND Industries 621 Heptane-Acetone SuperGlue accelerator Fast acting SuperGlue accelerator 15 seconds. Non-ozone depleting but flammable solvent |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | On Steel (Fixture) |
ND Industries SuperGlue Ethyl 395 General DescriptionA low viscosity ethyl-based cyanoacrylate that exhibits fast cure speeds on a wide range of common materials such as metals, rubbers, and plastics.Typical Usesloudspeaker componen.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Buna N Rubber, handling time |
Permabond 731 Cyanoacrylate, toughened PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6009 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6013 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6014 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | <= 0.250 min | <= 0.00417 hour | zinc, fixture time with initiator 44 |
Permabond TA459 Toughened Acrylic Adhesive Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens.. |
|||
Cure Time | 0.250 - 0.500 min | 0.00417 - 0.00833 hour | zinc, fixture time with initiator 43 |
Permabond TA459 Toughened Acrylic Adhesive Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens.. |
|||
Cure Time | 0.250 - 0.500 min | 0.00417 - 0.00833 hour | zinc, fixture time with initiator 44 |
Permabond TA4590 Toughened Acrylic Adhesive Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6602 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6813 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 0.250 min | 0.00417 hour | Steel, set time |
Permabond 200 Cyanoacrylate, wire tacking PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy.. |
|||
Cure Time | 0.250 min | 0.00417 hour | Phenolic, set time |
Permabond 200 Cyanoacrylate, wire tacking PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Phenolic, handling time |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6810 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6811 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | >= 0.250 min | >= 0.00417 hour | Fixture |
Resinlab® CYNERGY CA6812 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 0.250 min | 0.00417 hour | |
Loctite® 406 Surface Insensitive Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Cure Time | 0.250 min | 0.00417 hour | |
Loctite® 412 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Cure Time | 0.250 min | 0.00417 hour | |
Loctite® PRISM® 454 Instant Adhesive Gel Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Cure Time | <= 0.250 min | <= 0.00417 hour | |
Dymax 957 Potting and Encapsulation Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 957 Potting and Encapsulation AdhesiveDesigned to adhere to a wide variety of materials, high strength. Cure Type: U.. |
|||
Cure Time | 0.250 - 1.00 min | 0.00417 - 0.0167 hour | |
3M Scotch-Weld™ CA5 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Higher viscosity, slower setting version of CA4 for filling gaps. Meets CID A-A-3097, Type II, Clas.. |
|||
Cure Time | 0.250 min | 0.00417 hour | Set Time |
3M Scotch-Weld™ EZ250015 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w.. |
|||
Cure Time | 0.250 - 0.667 min | 0.00417 - 0.0111 hour | Time to Handling Strength |
3M Scotch-Weld™ HT700 High Temperature Instant Adhesive 3M™ Scotch-Weld™ High Temperature Instant Adhesives provide superior performance for demanding applications where high temperatures, thermal cycling, or shock resistance is required. HT700 is a me.. |
|||
Cure Time | 0.250 - 0.583 min | 0.00417 - 0.00972 hour | Time to Handling Strength |
3M Scotch-Weld™ SI5 Surface Insensitive Instant Adhesive 3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI5 (formerly SB20) is a very l.. |
|||
Cure Time | 0.250 - 0.333 min | 0.00417 - 0.00556 hour | Fixture Rate |
Dymax Magnet Bonder™ 2000 Adhesive DYMAX® Magnet Bonder™ Adhesives for Higher Performance and Lower CostDymax 2000 Magnet Bonder™ AdhesiveFastest cure; bond ferrite to steel. Typical Use: Loudspeaker magnet to pole piece. |
|||
Cure Time | 0.250 - 0.417 min | 0.00417 - 0.00694 hour | Per 1 mm of wall thickness, injection molding |
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U.. |