Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Vyram™ 9101-65 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Stellarchem 8075 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Stellarchem FP-860 TPE Compound Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Stellarchem GP-965B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Stellarchem SE/PA745B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Stellarchem SV-B80E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Stellarchem SV-B87E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Screw Speed | 50 - 200 rpm | 50 - 200 rpm | |
Teknor Apex Beetle® 66GS6 Nylon 66, 30% Glass Bead Reinforced Notes: 66GS6 is a 30% glass sphere filled nylon 66 that offers increased rigidity coupled with low distortion Features: High Rigidity; Low Warpage Processing Method: Injection Molding Forms: Pellet.. |
|||
Screw Speed | 50 - 200 rpm | 50 - 200 rpm | |
Teknor Apex Beetle® MDF2 Nylon 6, 30% Short Glass Fiber Reinforced, Dry Notes: MDF2 is a heat stabilized 30% glass fiber reinforced nylon 6 that offers good mechanical performance coupled with good surface finish. Features: Heat Stabilized; Good Surface Finish Processin.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
Teknor Apex Sarlink® 4445 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4445 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Screw Speed | 160 - 200 rpm | 160 - 200 rpm | |
Lubrizol Estane® S364D Thermoplastic Polyurethane Type: Estane® S364D is a Shore 65D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Screw Speed | 160 - 200 rpm | 160 - 200 rpm | |
Lubrizol Estane® T465A Thermoplastic Polyurethane Type: Estane® T465A is a Shore 71A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor.. |
|||
Screw Speed | 50 - 200 rpm | 50 - 200 rpm | |
Topas Advanced Polymers TOPAS® 6013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6013S-04 is a general purpose injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance,.. |
|||
Screw Speed | 50 - 200 rpm | 50 - 200 rpm | |
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Santoprene® 121-50M100 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult .. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Santoprene® 201-87 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection |
Alliance Polymers Viprene™ G45D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G45D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection |
Alliance Polymers Viprene™ G75A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G75A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection |
Alliance Polymers Viprene™ G85A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G85A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection |
Alliance Polymers Viprene™ G90A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection |
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
Alliance Polymers Zythane™ 4050D Thermoplastic Polyurethane Elastomer Zythane™ 4050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
Alliance Polymers Zythane™ 5080A Thermoplastic Polyurethane Elastomer Zythane™ 5080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer Zythane™ 7090A is a polyether-based TPU specifically formulated for extrusion molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good hydroly.. |
|||
Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
ExxonMobil Santoprene® 211-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Screw Speed | 160 - 200 rpm | 160 - 200 rpm | |
Lubrizol Estane® T865A Thermoplastic Polyurethane Type: Estane® T865A is a Shore 71A, polyester grade, plasticized low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Corporation |