Processing Properties Metric English Comments
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 241-80 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Vyram™ 9101-45 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Vyram™ 9101-85 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Vyram™ 9103-45 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Stellarchem AB855LG TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Stellarchem AB870EM TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Stellarchem FP-860 TPE Compound
Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Stellarchem GP-965B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Stellarchem LP-830 TPE Compound
This grade of Stellarchem LP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, ..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Stellarchem SV-B65E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Stellarchem MP-855WR TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer
A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3160 can be processed by injection molding or extrusion for ap..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 251-70W232 Thermoplastic Elastomer
A soft, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer
A hard, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Screw Speed <= 100 rpm
<= 100 rpm
Beijing Ranger Chem PBT-201-G10 202 Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection
Alliance Polymers Viprene™ G85A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G85A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection
Alliance Polymers Viprene™ P70A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P70A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Screw Speed <= 100 rpm
<= 100 rpm
Beijing Chemical Industry KAIFA® 301-G20 PBT Resin
20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Screw Speed <= 100 rpm
<= 100 rpm
Beijing Ranger Chem PBT-201-G10 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Screw Speed <= 100 rpm
<= 100 rpm
BLUESTAR PBT 403M-G20 20% Glass Filled
PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by Polymer Technology and Services, LLC (PTS).
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 221-87 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 101-73 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Screw Speed 100 - 200 rpm
100 - 200 rpm
to be chosen in such a way that plasticizing time is just within cooling time
Gromax CCP PET 9130-200 30% Glass Filled
Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell..
Copyright © lookpolymers.com All Rights Reserved