POLYMER SEARCH
Polymer Property : Back Pressure = 435 psi
Polymer Property :
Back Pressure =
435 psi
Product List
Processing Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties
Metric
English
Comments
Back Pressure
3.00
-
5.00
MPa
435
-
725
psi
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Dry