Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 150 - 170 °C | 302 - 338 °F | Always recommended, temperature can be reduced when using vacuum ovens. |
LATI LARPEEK 10 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Drying Temperature | 150 - 170 °C | 302 - 338 °F | Always recommended, temperature can be reduced when using vacuum ovens. |
LATI LARPEEK 10 K/20 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Drying Temperature | 150 - 170 °C | 302 - 338 °F | Always recommended, temperature can be reduced when using vacuum ovens. |
LATI LARPEEK 10 K/40 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Drying Temperature | 150 - 170 °C | 302 - 338 °F | Always recommended, temperature can be reduced when using vacuum ovens. |
LATI LARPEEK 50 K/30 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Drying Temperature | 150 °C @Time 10800 sec |
302 °F @Time 3.00 hour |
|
Victrex® Vicote® 702 Polyetheretherketone (PEEK) Powder Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail.. |
|||
Drying Temperature | 150 °C | 302 °F | |
Hybrid Plastics PO6C81.01 Nanoreinforced® Polyphenylene Oxide (PPO) PPO available on the market today is typically mixed with polystyrene or other polymers to make it processable. However, these resins degrade the excellent mechanical and flammability properties of .. |
|||
Drying Temperature | 150 °C @Time 14400 sec |
302 °F @Time 4.00 hour |
|
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK) AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. .. |
|||
Drying Temperature | 150 °C @Time 10800 sec |
302 °F @Time 3.00 hour |
|
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU), 20% Glass Fiber Veradel® 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Drying Temperature | 150 °C @Time 14400 sec |
302 °F @Time 4.00 hour |
|
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Drying Temperature | 150 °C | 302 °F | overnight |
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H.. |
|||
Drying Temperature | 150 - 160 °C | 302 - 320 °F | |
Eastman Eastar EN063 Polyester Eastar Polyester EN063 is a condensation polymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Eastar Polyester EN063 is a homopolymer .. |
|||
Drying Temperature | 150 °C | 302 °F | |
Eastman Eastar EN076 Copolyester Eastar Copolyester EN076 is recommended for the thick-walled containers that are prevalent in the cosmetics and personal care markets. This copolyester offers good processability with the benefits o.. |
|||
Drying Temperature | 150 - 180 °C @Time 10800 sec |
302 - 356 °F @Time 3.00 hour |
|
LATI Lapex A G/30 PES, 30% Glass Fiber Reinforced Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Drying Temperature | 150 °C @Time 10800 sec |
302 °F @Time 3.00 hour |
|
Victrex® Vicote® 701 Polyetheretherketone (PEEK) Powder Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail.. |