Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 50.0 - 55.0 °C @Time >=10800 sec |
122 - 131 °F @Time >=3.00 hour |
If stored for longer than 1 year |
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **) PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |