Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 120 - 140 °C | 248 - 284 °F | |
PTS PBT-6630 30% Glass Filled PBT6630 is an injection molding grade, with 30% glass fiber reinforced, high heat stability, and electrical properties, easy to process. It is widely used in automotive, home appliance, Electrical i.. |
|||
Drying Temperature | 100 - 140 °C | 212 - 284 °F | Injection Molding |
DuPont Performance Polymers Crastin® CE15330 NC010 PBT
(Unverified Data**) Crastin® CE15330 NC010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Drying Temperature | 120 - 140 °C @Time 10800 - 18000 sec |
248 - 284 °F @Time 3.00 - 5.00 hour |
Pre-dry |
Kingfa PBT-T30 30% Mineral Filled PBT Features:Excellent size stabilityLow tendency to wrapLow abrasionGood surfaceApplications:Injection moldingApplication partsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Drying Temperature | 120 - 140 °C | 248 - 284 °F | Injection Molding |
LG Chemical LUCON SP9306FL sPS+MF Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 .. |
|||
Drying Temperature | 120 - 140 °C @Time 10800 - 18000 sec |
248 - 284 °F @Time 3.00 - 5.00 hour |
Pre-dry |
Kingfa PET-G15 15% Glass Fiber Reinforced PET Features:High strengthGood heat resistanceApplications:Injection moldingApplication partsAuto partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Drying Temperature | 120 - 140 °C | 248 - 284 °F | |
Eurotec® Tecopet® PT70 GR30 NL100 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Drying Temperature | 130 - 140 °C | 266 - 284 °F | Temperature can be reduced when using vacuum ovens. |
LATI LARTON G/30 30% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Drying Temperature | 116 - 140 °C | 240 - 284 °F | Average value: 124 °C Grade Count:8 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |