Polymer Property : Drying Temperature = 165 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 165 - 177 °C

@Time 14400 sec
329 - 351 °F

@Time 4.00 hour
Solvay Specialty Polymers Radel® R-7120 Polyphenylsulfone, 20% glass fiber  (discontinued **)
RADEL R 7120 is a 20% glass fiber reinforced grade of RADEL R polyphenylsulfone developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 ..
Copyright © lookpolymers.com All Rights Reserved