Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 192 - 215 °C | 378 - 419 °F | Start Point: 200°C |
Kingfa FRHIPS-702 Flame Retardant Polystyrene Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing.. |
|||
Rear Barrel Temperature | 175 - 215 °C | 347 - 419 °F | Blow Molding |
LG Chemical HYPERIER IP1306B PA-HDPE Nanoclay Compound HYPERIER is a nano compound made from nano-sized inorganic plate clay. Blow Molding, Barrier thermoplastic, Nylon blend with HDPEApplication: Agrochemical Container, SORE* Fuel Tank, PFCCAS No. 900.. |
|||
Rear Barrel Temperature | 192 - 215 °C | 378 - 419 °F | Start Point: 200°C |
Kingfa FRHIPS-722 Flame Retardant Polystyrene Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing.. |